Fusible interlining, when applied correctly, gives a garment a shape that lasts for years; when applied incorrectly, it delaminates in the wash, bubbles up or damages the fabric. The secret lies in three key parameters: heat, pressure and time.
How does fusible interlining work?
One side of fusible interlining is coated with dots of heat-activated adhesive resin. When heat is applied, this resin melts; under pressure it penetrates the fibres of the fabric; and once the heat is removed and it cools, the fabric and the interlining bond permanently.
The three key parameters
- Heat (temperature): The correct temperature needed to melt the resin. Too low and it won't bond; too high and the fabric glazes or the interlining is damaged.
- Pressure: Ensures the melted resin penetrates the fabric. Insufficient pressure leads to a weak bond.
- Time: The duration for which heat and pressure must be applied. Too short means incomplete bonding; too long means fabric damage.
These three values vary depending on the interlining and fabric used. The safest approach is to consult your interlining supplier for the correct settings.
Choose the right interlining for your application
Every fabric and every machine calls for a different interlining. Browse the range of interlinings suited to your application at Online Tela; if you're not sure, our expert team will guide you.
Browse the Online StoreApplying with an iron (step by step)
- Place the adhesive (rough/dotted) side of the interlining against the reverse side of the fabric.
- Place a thin cloth (pressing cloth) in between; press down with the iron without sliding it.
- At the correct temperature, apply equal pressure and time to every area.
- Do not move the fabric until it has cooled; the bond completes as it cools.
Industrial application: fusing press machine
In mass production, interlining is applied with a fusing press machine. The machine controls heat, pressure and time in a standardised, repeatable way, ensuring the same quality in every batch. This is exactly the principle of consistency that Telpa values: the same technical specification in every roll we supply.
Common mistakes
- Choosing the wrong interlining (e.g. paper/nonwoven interlining in shirts) — it delaminates after a few washes.
- Insufficient pressure or time — the interlining bubbles and blisters.
- Excessive temperature — the fabric glazes and the resin strikes through to the fabric surface.
Wash resistance
The right interlining + the right application = a long service life. For frequently washed shirts in particular, using a wash-resistant, specially coated woven shirt interlining is essential. Cheap paper (nonwoven) interlining should be avoided in shirts, as it causes problems after 3–5 washes.